Chasing the hydrogen-saturated defects in tungsten with Muon spectroscopy

DOI

The structure and dynamics of hydrogen (H) defects in tungsten recently become a topic of major interest since this metal has been chosen as shielding material for the next step fusion device ITER.With the help of muon spin relaxation and rotation, which are not limited by the dilution of H, we plan to explore samples specifically prepared with proton irradiation or Si/W ion implantation to have different damage profiles in terms of mono-vacancies and larger clusters.Ultimately, the object of our study is to obtain further understanding of the location of H and of its behaviour in tungsten, starting from low temperatures, where a static muon will mimic H trapped in materials' defects, up to several hundred degrees, where dynamics will take place after the release of H from the trapping sites.

Identifier
DOI https://doi.org/10.5286/ISIS.E.90598260
Metadata Access https://icatisis.esc.rl.ac.uk/oaipmh/request?verb=GetRecord&metadataPrefix=oai_datacite&identifier=oai:icatisis.esc.rl.ac.uk:inv/90598260
Provenance
Creator Professor Jyrki Räisänen; Dr Stephen Cottrell; Dr Matteo Aramini; Professor Filip Tuomisto
Publisher ISIS Neutron and Muon Source
Publication Year 2021
Rights CC-BY Attribution 4.0 International; https://creativecommons.org/licenses/by/4.0/
OpenAccess true
Contact isisdata(at)stfc.ac.uk
Representation
Resource Type Dataset
Discipline Natural Sciences; Physics
Temporal Coverage Begin 2018-02-15T09:30:00Z
Temporal Coverage End 2018-03-02T08:33:21Z