5 datasets found

Keywords: Chemical Engineering Design

Filter Results
  • 3D Dendritic Microstructure (1 mA)

     The Zn||separator||Zn Swagelok cell was scanned in the fresh state as well as after 120-minutes electrodeposition under two different currents (1 mA) using a Nikon XTH 225...
  • 3D Dendritic Microstructure (0.1 mA)

    The Zn||separator||Zn Swagelok cell was scanned in the fresh state as well as after 120-minutes electrodeposition under two different currents (0.1 mA) using a Nikon XTH 225...
  • Formation of Zn Dendrites (6 mA)

    Operando observation of dynamic dendritic formation and dissolution within the symmetric Zn||Zn cell was performed with a 4K digital microscope (Keyence VHX-7000, Japan). A 50×...
  • Formation of Zn Dendrites (6 mA & 1 mA)

    Operando observation of dynamic dendritic formation and dissolution within the symmetric Zn||Zn cell was performed with a 4K digital microscope (Keyence VHX-7000, Japan). A 50×...
  • Formation of Zn Dendrites (10 mA)

    Operando observation of dynamic dendritic formation and dissolution within the symmetric Zn||Zn cell was performed with a 4K digital microscope (Keyence VHX-7000, Japan). A 50×...